Polymers obtained from renewable sources are gaining popularity over their petroleum based counter parts in recent years due to their capability to address the environmental pollution related concerns emanating from the widespread usage of synthetic polymers. Even though the polymers from renewable sources are attractive in an environmental point of view, some of the property limitations and the high cost of these materials pose limitations for their extensive commercial applications. These aspects opened the door for a large chunk of research activities in development of polyblends and composites containing polymers from renewable sources as one of the components. Poly (lactic acid) (PLA) is one of the most discussed and commercialized polymer originated from renewable resources. Even though it has many useful properties, certain disadvantages like high brittleness, low impact resistance etc. limit the wide spread commercialization of PLA. In this review article, the recent research activities which are aimed to fill this gap by various modifications of PLA are discussed with special emphasis on the latest research advancements in the field of biodegradable and non biodegradable systems containing PLA.
The development of flexible, wearable electronic devices is one of the future directions of technology development. Flexible conductive materials are important supporting materials for wearable electronic devices. Polymer has excellent flexibility; it is an important way to prepare flexible conductors from polymer-based conductive composites. In this paper, the research progress of polymer-based flexible conductive composites is summarized in terms of preparation and characterization methods. The key factors to realize flexible conductors are put forward, namely, the maintenance of excellent polymer elasticity and the realization of stability. The design and preparation of the extensible conductor with high-elasticity matrix and nanofiller are introduced in detail, and the problems in the current research are summarized.
The nylon 66/nano-CaCO3 composites were prepared by melt blending on a twin-screw extruder. Scanning electron microscopy (SEM), polarized light microscopy (PLM), thermal loss (TGA) and differential scanning calorimetry (DSC) The effects of nanometer calcium carbonate on the polycrystalline behavior and thermal properties of nylon 66/nano CaCO3 composites were investigated. The results show that the nanometer calcium carbonate particles are dispersed in the nylon 66 matrix and exist in the form of aggregates. The nanometer calcium carbonate has the effect of heterogeneous nucleation, which can reduce the size of the spherules. The decomposition temperature of the nylon 66 is 400 ℃, the addition of nano-CaCO3 to reduce the decomposition temperature. At the same time, DSC test showed that the β-crystalline form in the material reduced the melting temperature of the material. The addition of nano-CaCO3 in the nylon 66 matrix resulted in the decrease of the crystallization temperature and the increase of the half-height width of the endothermic peak. The lower the crystallization temperature, the wider the crystallization temperature range.
Lead sulfide (PbS) is an important IV-VI semiconductor material with narrow bandwidth and wide wave width, which attracts people's attention. Nano-level PbS has many novel optoelectronic properties and has a wide range of applications in the field of optoelectronics, such as infrared optoelectronic devices, photovoltaic devices, light-emitting devices and display devices. In this paper, Pbs is produced by solvent thermal method by using lead acetate as lead source, sulfur power as sulfur source, ethylene glycol as solvent, and acetic acid to provide acidic environment. The reaction acidity, type of lead source, amount of sulfur source and other aspects will be explored. The products obtained under different conditions were characterized by X-ray diffraction (XRD), optical microscopy and scanning electron microscopy (SEM). The results showed that PbS produced at 140°C for 24 hours, using 14mL ethylene glycol and 1.2mL acetic acid has the best morphology. It has a non-planar six-arm symmetrical structure. Finally, we prepare the lead sulfide composite Ni/PbS, and characterized it.
Copyright © by EnPress Publisher. All rights reserved.